Trying to see if this is something that happens normally, our emulsion has millions of little bubbles. I added diazo when we first got it, and let it sit for more than 12 hours before I used it. Anyone else have this problem? When coating screens it's leaving little airpockets, especially on 110 mesh. If I coat slow enough they aren't visible on higher mesh, but 110 they are very visible and I am worried about pinholes and whatnot. Any advice would be helpful! Thanks.

Sidenote: We just switched from using SP1400 because we were getting build up of ink on larger color jobs, seemed to be the emulsion causing that.